MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Specialty Compounds RTP Company
SACO AEI THERMODAN® HF TP-0812 Thermoplastic, low smoke, halogen free, flame retardant compound for cable insulation and sheathing
Categories: Polymer; Thermoplastic

Material Notes: THERMODAN® HF TP-0812 is a flame retardant, low smoke, thermoplastic compound, which has been specifically developed for excellent processing characteristics at high extrusion speeds making it suitable for telecom, data and general cable applications. It offers low shrink characteristics and is therefore suitable for use as fiber optic jacketing. THERMODAN® HF TP-0812 is capable of meeting the flame retardant requirements of UL 1666, UL 1685, IEEE 1202, FT-4 in specific fiber optic constructions. It is also recognized as halogen free under UL 2885. It can be extruded using PVC extruders and screws. It possesses excellent tensile and flame retardant properties and meets the requirements of limited toxic and corrosive fume emission.

Information provided by SACO AEI Polymers, Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Melt Flow, ASTM D1238
  • Storage Temperature
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength at Break, UL 2556
  • Tensile Strength at Break, UL 2556, after thermal ageing
  • Elongation at Break, UL 2556
  • Elongation at Break, UL 2556, after thermal ageing
  • Tear Strength, BS6469
  • Oxygen Index, ASTM D2863
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Die Temperature
  • Melt Temperature
  • Head Temperature
  • Drying Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Master Bond adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.