MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SACO AEI THERMODAN® HF TP-0812 Thermoplastic, low smoke, halogen free, flame retardant compound for cable insulation and sheathing
Categories: Polymer; Thermoplastic

Material Notes: THERMODAN® HF TP-0812 is a flame retardant, low smoke, thermoplastic compound, which has been specifically developed for excellent processing characteristics at high extrusion speeds making it suitable for telecom, data and general cable applications. It offers low shrink characteristics and is therefore suitable for use as fiber optic jacketing. THERMODAN® HF TP-0812 is capable of meeting the flame retardant requirements of UL 1666, UL 1685, IEEE 1202, FT-4 in specific fiber optic constructions. It is also recognized as halogen free under UL 2885. It can be extruded using PVC extruders and screws. It possesses excellent tensile and flame retardant properties and meets the requirements of limited toxic and corrosive fume emission.

Information provided by SACO AEI Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccASTM D792
Melt Flow 6.0 g/10 min
@Load 21.6 kg,
Temperature 150 °C
ASTM D1238
Storage Temperature <= 30.0 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 1800 psiUL 2556
 >= 2070 psi
@Treatment Temp. 100 °C,
Time 605000 sec
after thermal ageing; UL 2556
Elongation at Break 180 %UL 2556
 >= 135 %
@Treatment Temp. 100 °C,
Time 605000 sec
after thermal ageing; UL 2556
Tear Strength 40.0 pliBS6469
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 40 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 130 °C
Zone 2 150 °C
Zone 3 170 °C
Zone 4 180 °C
Die Temperature 190 °C
Melt Temperature 190 °C
Head Temperature 190 °C
Drying Temperature 60.0 °C
@Time 14400 - 21600 sec
Shelf Life 60.0 Month
 
Descriptive Properties
Acid Gas<5 mg/gIEC 60754-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO082 / 265512

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.