MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics Tecknit® 72-00008 Silver-Filled Epoxy System
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Description: This commercial grade, conductive epoxy is designed for use in bonding applications where good conductivity is required. When mixed in a ratio of 1:1.4 by volume or weight, the two components produce a light colored creamy paste which can be easily applied.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 6.89 MPaCured; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.020 ohm-cmCured; QAP-1017
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 149 °CCured
Minimum Service Temperature, Air -62.0 °CCured
Shrinkage <= 1.0 %Cured
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hour
@Temperature 100 °C
Recommended Cure
Pot Life 45 min
@Temperature 25.0 °C
Shelf Life 15.0 MonthUnopened Container
 
Descriptive Properties
ColorSilver Gray
ConsistencyThick Paste
FillerAg/Glass
Final ConditionRigid
Mix Ratio1:1.4
Number of ComponentsTwo
ResinEpoxy
Volume14.7 in3
Weight16 oz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics Tecknit® 0002 Highly Conductive Adhesive-Sealant Silver Silicone
Parker Chomerics Tecknit® 0036 Two Part Flexible Adhesive-Sealant Silver-Glass Silicone
Parker Chomerics Tecknit® 73-00008 Electrically Conductive Acrylic and Polyurethane Paint
Parker Chomerics Tecknit® 72-00152 Silver-Filled Flexible Resin Caulking System
Parker Chomerics Tecknit® 72-00151 Silver-Filled Flexible Resin Caulking System

PCHOME408 / 131118

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.