MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
AISI 1118 Steel, mock carburized at 925°C (1700°F) for 8 hours, 790°C (1450°F) reheat, water quenched, 175°C (350°F) temper, round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Low Carbon Steel

Material Notes: Applications include medium duty shafts, studs, pins, distributor cams, cam shafts, and universal joints.

Key Words: NS G11180, ASTM A29, ASTM A107, ASTM A108, FED QQ-S-637 (C1118), SAE J403, SAE J412, SAE J414
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/ccTypical for steel.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 156
@Diameter 102 mm
 167
@Diameter 50.8 mm
 207
@Diameter 25.4 mm
 285
@Diameter 12.7 mm
Hardness, Knoop 176
@Diameter 102 mm
Converted from Brinell
 188
@Diameter 50.8 mm
Converted from Brinell
 229
@Diameter 25.4 mm
Converted from Brinell
 311
@Diameter 12.7 mm
Converted from Brinell
Hardness, Rockwell B 82
@Diameter 102 mm
Converted from Brinell
 85
@Diameter 50.8 mm
Converted from Brinell
 93
@Diameter 25.4 mm
Converted from Brinell
 99
@Diameter 12.7 mm
Converted from Brinell
Hardness, Rockwell C 15
@Diameter 25.4 mm
Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
 30
@Diameter 12.7 mm
Converted from Brinell
Hardness, Vickers 163
@Diameter 102 mm
Converted from Brinell
 175
@Diameter 50.8 mm
Converted from Brinell
 217
@Diameter 25.4 mm
Converted from Brinell
 301
@Diameter 12.7 mm
Converted from Brinell
Tensile Strength, Ultimate 531 MPa
@Diameter 102 mm
 567 MPa
@Diameter 50.8 mm
 707 MPa
@Diameter 25.4 mm
 996 MPa
@Diameter 12.7 mm
Tensile Strength, Yield 310 MPa
@Diameter 102 mm
 330 MPa
@Diameter 50.8 mm
 409 MPa
@Diameter 25.4 mm
 621 MPa
@Diameter 12.7 mm
Elongation at Break 13.2 %
@Diameter 12.7 mm
in 50 mm
 19 %
@Diameter 25.4 mm
in 50 mm
 27.3 %
@Diameter 50.8 mm
in 50 mm
 31 %
@Diameter 102 mm
in 50 mm
Reduction of Area 30.8 %
@Diameter 12.7 mm
 48.9 %
@Diameter 25.4 mm
 65.5 %
@Diameter 50.8 mm
 67.4 %
@Diameter 102 mm
Modulus of Elasticity 200 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel.
Poissons Ratio 0.29Typical For Steel
Shear Modulus 80.0 GPaTypical for steel.
Izod Impact 103 Jnormalized at 925°C (1700°F)
 107 Jannealed at 790°C (1450°F)
 108 Jas rolled
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000174 ohm-cmTypical steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 20.0 °C
Typical steel
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
Typical for steel
 13.9 µm/m-°C
@Temperature 0.000 - 500 °C
Typical for steel
Specific Heat Capacity 0.472 J/g-°CTypical steel
Thermal Conductivity 51.9 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.14 - 0.20 %
Iron, Fe 98.03 - 98.48 %As remainder
Manganese, Mn 1.3 - 1.6 %
Phosphorus, P <= 0.040 %
Sulfur, S 0.080 - 0.13 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1118 Steel, normalized at 925°C (1700°F), air cooled, round
AISI 1117 Steel, mock carburized at 925°C (1700°F) for 8 hours, 790°C (1450°F) reheat, water quenched, 175°C (350°F) temper, round
AISI 1118 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1137 Steel, water quenched from 845°C (1550°F), 540°C (1000°F) temper, round
AISI 1045 Steel, as cold drawn, 50-75 mm (2-3 in) round

M1118W / 7176

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.