MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Envalior Arnitel® PL420-H TPC-ET, Injection Molding, Heat Stabilized
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE; Polyester, TP

Material Notes: Injection Molding, Heat Stabilized

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183
Melt Flow 23 g/10 min
@Load 2.16 kg,
Temperature 230 °C
MVR, [cm3/10min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 17.5 MPaISO 527-1/-2
Tensile Stress at Strain 5.30 MPa
@Strain 10 %
ISO 527-1/-2
 10.8 MPa
@Strain 100 %
ISO 527-1/-2
Elongation at Break 400 %Nominal; ISO 527-1/-2
Tensile Modulus 100 MPaISO 527-1/-2
Izod Impact, Notched (ISO) NB
@Temperature 23.0 °C
ISO 180/1A
 NB
@Temperature -30.0 °C
ISO 180/1A
Charpy Impact, Notched NB
@Temperature 23.0 °C
ISO 179/1eA
 NB
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °C10°C/min; ISO 11357-1/-3
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 HB
@Thickness 3.00 mm
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer
Envalior Arnitel® PB420 TPC-ET
Celanese Hytrel® HTR237BG BK320 TPC-ET
Envalior Arnitel® EB463 TPC-ET, Blow Molding Grade
Celanese SO.F.TER Pibiflex® B 5050 MWR NERO Copolyester TPE

PDSM8122 / 184823

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.