MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese SO.F.TER Pibiflex® B 5050 MWR NERO Copolyester TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Blow Molding Thermoplastic Copolyester Elastomer

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
0.60 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4141ASTM D2240
Tensile Strength 30.0 MPa4350 psiASTM D638
Elongation at Break 460 %460 %ASTM D638
Flexural Modulus 0.0900 GPa13.1 ksiASTM D790
Izod Impact, Notched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256/A
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ASTM D256/A
Tear Strength 110 kN/m628 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Melting Point 200 °C392 °FASTM D3417
Vicat Softening Point 155 °C311 °F120°C/h at 10 N; ASTM D648
Oxygen Index 20 %20 %ASTM D2863
 
Descriptive Properties
Fatigue Resistance (mm/1000 cycles).1/300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Arnitel® EB463 TPC-ET, Blow Molding Grade
Envalior Arnitel® EB464 TPC-ET, Blow Molding Grade
Celanese Hytrel® HTR8223 BK320 TPC-ET
Celanese Hytrel® HTR237BG BK320 TPC-ET
Envalior Arnitel® PB420-B TPC-ET

PSOFS787 / 162251

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.