MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AdvanSource Biomaterials HydroMed™ D640 Permanently Lubricious Polyurethane Coating
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: AdvanSource Biomaterials Corporation manufactures and markets hydrophilic high slip, high water absorptive, polyether hydrophilic polyurethanes designed for use as coatings of catheters, sutures, introducers, rods, valves and rubber products. HydroMed 640™ can also be coated onto silicon microdevices to reduce absorption of white cells and proteins on the devices, thereby aiding in the analysis of blood and DNA.

HydroMed 640™ is processed by traditional solvent coating methods. The polymer granules are dissolved at 1-3% concentration in 95/5 ethanol/water or other organic solution. The catheter part is dipped into the solution for about three to about twenty seconds. Most of the solvent is evaporated at room temperature in about five to thirty minutes, the device is heated in an oven to 80º for about two to fifteen minutes, depending on coating thickness, to remove the solvent. For small batches, the polymer can be mixed with the solvent on a roller mill to dissolve the polymer. To prepare films of the polymer, a 10% solution is cast into an open mold and the solvent is evaporated at 80 C.

Information provided by AdvanSource Biomaterials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 - 1.17 g/cc
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.048
 
Thermal PropertiesOriginal ValueComments
Softening Point 230 - 270 °F
 
Descriptive Properties
Linear Expansion1.15
Water Content0.9

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AdvanSource Biomaterials HydroSlip™ C Hydrophilic Polyether Aliphatic Polyurethane
ATI Allvac® Vasco® 316-L Specialty Steel, Heat Treatment: 1038°C (1900°F) Anneal
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane
AdvanSource Biomaterials ChronoFlex® C 75D Biodurable Medical Grade Polyurethane
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer

PCARDI10 / 27934

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.