MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LATI Larton CE/60 PPS, 60% Mineral Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Polyphenylene Sulfide (PPS) based compound. Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.87 g/cc
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
Linear Mold Shrinkage, Transverse 0.0030 - 0.0060 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPa
@Temperature 150 °C
 35.0 MPa
@Temperature 120 °C
 55.0 MPa
@Temperature 90.0 °C
 65.0 MPa
@Temperature 60.0 °C
 70.0 MPa
@Temperature 23.0 °C
Elongation at Break 0.50 %
@Temperature 23.0 °C
 0.80 %
@Temperature 60.0 °C
 1.2 %
@Temperature 90.0 °C
 1.7 %
@Temperature 120 °C
 1.9 %
@Temperature 150 °C
Tensile Modulus 4200 MPa
@Temperature 150 °C
 7600 MPa
@Temperature 120 °C
 9100 MPa
@Temperature 90.0 °C
 9900 MPa
@Temperature 60.0 °C
 11500 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 5.00 kJ/m²
Charpy Impact, Notched 2.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
Vicat Softening Point 250 °C
@Load 5.00 kg
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
Oxygen Index 44 %
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 - 330 °C
Mold Temperature 130 - 140 °C
Drying Temperature 130 - 150 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese FORTRON 6160B4 PPS, 60% Mineral / Glass Reinforced
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced
Celanese FORTRON 300 PPS, Unfilled
Celanese Fortron® 4184 L4 Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
DuPont Mobility and Materials Delrin® 570 NC000 POM-GF20

PLATH9648 / 177344

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.