MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese FORTRON 300 PPS, Unfilled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: This grade designation represents a series of Fortron PPS grades used for extruding various shapes like Rod and Slab. These grades are the stiffest flowing unfilled products offered. For extrusion applications requiring a PPS grade with glass reinforce
FORTRON should in principle be predried. Because of the necessary low maximum residual moisture content the use of dry air dryers is recommended. The dew point should be =< - 30° C. The time between drying and processing should be as short as possible.
For subsequent storage the material should be stored dry in the dryer until processed (<= 60 h).

Information provided by Celanese Corporation.

Key Words: Extrusion Grade
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Density 1.316 g/cc0.04754 lb/in³ISO 1183
 1.40 g/cc0.0505 lb/in³ASTM D792
Water Absorption 0.030 %
@Temperature 22.8 °C
0.030 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9393ASTM D785
Tensile Strength at Break 86.2 MPa
@Temperature 22.8 °C
12500 psi
@Temperature 73.0 °F
ASTM D638
Elongation at Break 3.0 %
@Temperature 22.8 °C
3.0 %
@Temperature 73.0 °F
ASTM D638
Tensile Modulus 2.82 GPa409 ksi1mm/min; ISO 527-2/1A
Flexural Strength 145 MPa
@Temperature 22.8 °C
21000 psi
@Temperature 73.0 °F
ASTM D790
Flexural Modulus 2.47 GPa358 ksiISO 178
 4.14 GPa
@Temperature 22.8 °C
600 ksi
@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 0.267 J/cm
@Temperature 22.8 °C
0.500 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
@Temperature 22.8 °C
6.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Notched (ISO) 4.90 kJ/m²2.33 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched 8.91 J/cm²42.4 ft-lb/in²ISO 179/1eU
 22.61 J/cm²
@Temperature -30.0 °C
107.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.460 J/cm²2.19 ft-lb/in²ISO 179/1eA
 0.440 J/cm²
@Temperature -30.0 °C
2.09 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 ohm-cm1.00e+9 ohm-cmIEC 60093
 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant  2.7
@Frequency 10000 Hz
2.7
@Frequency 10000 Hz
IEC 60250
 2.8
@Frequency 1e+6 Hz
2.8
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 1000 Hz
3.0
@Frequency 1000 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 38.0 kV/mm965 kV/inIEC 60243-1
Dissipation Factor  0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
IEC 60250
 0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 124 sec124 secASTM D495
Comparative Tracking Index 125 V125 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 53.0 µm/m-°C29.4 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 54.0 µm/m-°C30.0 µin/in-°FISO 11359-2
Melting Point 280 °C536 °FISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FISO 75-1, -2
 105 °C221 °FASTM D648
Deflection Temperature at 8.0 MPa 73.0 °C163 °FISO 75-1, -2
Glass Transition Temp, Tg 90.0 °C194 °FISO 11357-1,-2,-3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 30.0 °C68.0 - 86.0 °Fhopper
Melt Temperature 321 °C610 °FISO 294
Mold Temperature 135 °C275 °FISO 294
Injection Velocity 275 mm/sec10.8 in/secISO 294
Drying Temperature 110 - 120 °C230 - 248 °F
Dry Time 3 - 4 hour3 - 4 hour
Moisture Content 0.020 %0.020 %Necessary low maximum
Injection Pressure 83.0 MPa12000 psiISO 294
 
Descriptive Properties
Injection moldingNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 205 PPS, Unfilled
Celanese FORTRON 0203HS PPS, Unfilled
Celanese FORTRON 203 PPS, Unfilled
Celanese FORTRON 214 PPS, Unfilled
Celanese FORTRON 317 PPS, Unfilled

PHCS264 / 123679

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.