MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON PPS at temperatures below 392°F. Its low ionic impurities make it an excellent choice for applications where high purity is a concern. TECATRON GF40 is a glass reinforced material that offers extremely high strength along with excellent chemical resistance properties. TECATRON PVX is a bearing grade PPS that is suitable for high load applications.

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Density 0.0488 lb/in³ASTM D792
Water Absorption at Saturation 0.020 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 104ASTM D785
Tensile Strength, Yield 8700 psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break 4.0 %
@Temperature 22.8 °C
ASTM D638
Tensile Modulus 480000 psiASTM D638
Flexural Strength 17400 psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 435000 psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched 0.500 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Coefficient of Friction, Dynamic 0.24
@Pressure 0.276 MPa
50 fpm; ASTM D3702
K Factor (Wear Factor) 5.4e-8
@Pressure 0.276 MPa
(in3/hr)x(1/PV), 50 fpm, Against Steel; ASTM D3702
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz,
Temperature 22.8 °C
50% RH; ASTM D150
Dissipation Factor 0.00010
@Frequency 60 Hz,
Temperature 22.8 °C
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µin/in-°FASTM D696
Thermal Conductivity 2.08 BTU-in/hr-ft²-°F
Melting Point 540 °FASTM D2133
Maximum Service Temperature, Air 338 °FLong Term
Deflection Temperature at 0.46 MPa (66 psi) 400 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °FASTM D648
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS)
Albis Plastics Tedur® L V 9900-1 PPS, Unreinforced
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Overview of materials for Polyetherimide (PEI)
Mitsubishi Chemical Advanced Materials Duratron™ U2300 PEI Extruded 30% Glass Reinforced Polyetherimide

PENSIN035 / 92852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.