MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solvay FM® 377S Adhesive Film, psf 0.06 (293 gsm)
Categories: Polymer; Adhesive; Film; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: FM® 377 film adhesive is a 350°F (177°C) cure modified epoxy designed for continuous services at 350°F (177°C). FM 377 film adhesive provides outstanding durability in bonding metallic and non-metallic substrates, and in the co-cure or secondary bonding of composites structures. FM 377 adhesive exhibits excellent structural performance from -67°F to 350°F (-55°C to 177°C). FM 377 adhesive is manufactured as a supported film with a knit carrier or as an unsupported film. The unsupported version can be easily reticulated on honeycomb core or perforated metal.

Features & Benefits:

  • Designed for bonding metallic, non-metallic and sandwich structures
  • Excellent combination of high peel strength and high 350°F (177°C) shear strength
  • Designed for continuous service at 350°F (177°C)
  • Superior performance in co-cure or secondary bonding of composite structures
  • Easily reticulated on core or perforated metal for nacelle bonding applications
  • 30 days shop life at 75°F (24°C)
Applications:
  • Bonding metallic, non-metallic and sandwich structures
  • Co-cure and secondary bonding of composite structures

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %<= 1.0 %
Storage Temperature -18.0 °C-0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  13.6 MPa
@Temperature 177 °C
1970 psi
@Temperature 351 °F
Blister, Metal-to-Metal
 14.1 MPa
@Temperature 177 °C
2050 psi
@Temperature 351 °F
Blister, after 1000 hrs at 350°F, Metal-to-Metal
 24.72 MPa
@Temperature -55.0 °C
3585 psi
@Temperature -67.0 °F
Blister, Metal-to-Metal
 25.9 MPa
@Temperature 24.0 °C
3760 psi
@Temperature 75.2 °F
Blister, Metal-to-Metal
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C351 °Fcontinuous
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorGrey
Metal-to-Metal Climbing Drum Peel125 Nm/mMetal-to-Metal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elantas Conap FR-1046 / EA-02 Conapoxy® Resin / Conacure® Hardener
Solvay VTF 261 Film
Solvay VTA® 260 Adhesive Film
Solvay Thornel® T-605/50X 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor

PCYTED119 / 180421

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.