MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond Supreme 10HTCL Epoxy for Cryogenic Applications
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Supreme 10HTCL features a blend of performance properties including both high shear and peel strengths along with convenient handling. This one component system is formulated to cure at elevated temperatures, e.g. 60-75 minutes at 250°F, shorter times can be achieved at higher temperatures. Tensile shear strengths of 3,500 psi and T-peel strengths of over 30 pli are readily obtained. Supreme 10HTCL has a number of processing advantages; no mixing is necessary prior to use, the viscosity remains constant with time (i.e. it will not thicken over time), the working life is unlimited at room temperature, and the material is room temperature storable. It is cryogenically serviceable and has a wide temperature range of 4K to +400°F. Master Bond Supreme 10HTCL readily withstands severe thermal cycling along with mechanical shock and vibration. It is very resistant to many chemicals including water, oils, fuels, solvents, acids and bases. It has excellent adhesion to metals, glass, ceramics and many plastics. The cured epoxy is a superior electrical insulator. Its natural color is amber, but other colors are available. Supreme 10HTCL has a higher viscosity but flows nicely and can be easily applied to substrates. Supreme 10HTCL’s high performance properties coupled with its convenient handling make it widely used in a variety of applications in the aerospace, electronic, electrical, computer, metalworking, appliance, automotive and chemical industries.

Product Advantages:

  • Single component system; no mixing needed prior to use, no viscosity changes over time.
  • Room temperature storable.
  • Versatile cure schedules; 60-75 minutes at 250°F; 35-40 minutes at 300°F.
  • High shear and peel strengths to a wide variety of similar and dissimilar substrates.
  • Service temperature range of 4K to +400°F.
  • Good electrical insulating properties and chemical resistance.
  • Superior thermal cycling ability; resistance to mechanical and thermal shocks.
  • Excellent flow properties.
  • 100% reactive; contains no solvents or diluents.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 140000 - 200000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 70
Tensile Strength at Break >= 9500 psi
Elongation at Break >= 5.0 %
Tensile Modulus >= 400000 psi
Compressive Strength >= 9000 psi
Shear Strength >= 3500 psiTensile, Al to Al
Peel Strength 25.0 - 30.0 pliT-peel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Minimum Service Temperature, Air -270 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.583 - 0.667 hour
@Temperature 149 °C
 1.00 - 1.25 hour
@Temperature 121 °C
Shelf Life 3.00 - 6.00 Month
@Temperature 23.9 °C
in original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
Master Bond Supreme 10HTND-3 Non-Drip Epoxy Resists High Temperatures
Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F
Master Bond EP42HT-2Med Epoxy Meets USP Class VI Requirements
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization

PMASTB344 / 149591

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.