MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Polymer System Supreme 10HTFL features a blend of physical properties including outstanding peel strength, very high shear strength and a wide service temperature range of 4K to +350°F making it suitable for cryogenic applications. Supreme 10HTFL features highly desirable handling properties including no mixing and unlimited working life at room temperature. It should be noted that this one part epoxy requires a curing temperature of 250°F or above. Supreme 10HTFL has a blend of advantageous physical and mechanical properties. It is a forgiving epoxy, i.e. far less rigid than typical high temperature resistant epoxies. Supreme 10HTFL also allows for resistance to impact, thermal and mechanical shock and vibration, and is well suited for rigorous thermal cycling. The adhesive is often used when bonding substrates with different coefficients of thermal expansion. It is 100% reactive and does not contain any diluents or solvents. Master Bond Polymer System Supreme 10HTFL’s chemical resistance is noteworthy, especially to water, oil, fuels and many solvents even upon prolonged exposure in hostile environments. It has excellent adhesion to metals, glass, ceramics, wood, and many rubbers and plastics. When cured, the epoxy is a very good electrical insulator. Its normal color is gray. A non-drip version called Supreme 10HTFLND-2 is available, which will not flow when cured. Master Bond Polymer System Supreme 10HTFL features high performance coupled with convenient handling making it widely used in a variety of applications in the aerospace, electronic, OEM, electrical, computer, metalworking and chemical industries.

Product Advantages:

  • Room temperature storable. Optimum shelf life obtained when refrigerated; do not freeze
  • Versatile fast cure schedules; 75-90 minutes at 250°F; 45-60 minutes at 300°F
  • High bond strength to similar and dissimilar substrates over the wide temperature range of 4K to over 350°F
  • Very good electrical insulating properties
  • Highly resistant to mechanical and thermal shock
  • 100% reactive — no volatiles present; thixotropic
Key Features
  • High peel and shear strength
  • Cryogenically serviceable
  • High temperature resistant
  • No mix, single component system
  • Unlimited working life at room temperature
  • Thermal cycling resistant

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
Viscosity 350000 - 700000 cP350000 - 700000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 45 - 6545 - 65
Tensile Strength at Break >= 34.5 MPa>= 5000 psi
Elongation at Break >= 50 %>= 50 %
Shear Strength >= 13.8 MPa>= 2000 psiTensile, Al to Al
Peel Strength >= 7.01 kN/m>= 40.0 pliTensile, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -168 °C-270 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  45.0 - 60.0 min
@Temperature 149 °C
0.750 - 1.00 hour
@Temperature 300 °F
 75.0 - 90.0 min
@Temperature 121 °C
1.25 - 1.50 hour
@Temperature 250 °F
Shelf Life 3.00 - 6.00 Month
@Temperature 23.9 °C
3.00 - 6.00 Month
@Temperature 75.0 °F
in original unopened containers
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy
Master Bond Supreme 10HTCL Epoxy for Cryogenic Applications
Master Bond EP51FL-1 Rapid Curing Cryogenic Two Component Epoxy
Master Bond EP45HTQ Quartz Filled Heat Resistant Epoxy

PMASTB345 / 149592

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.