MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
AGC AFLAS® 300S TFE/P Latex
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: AFLAS 300S Latex is an alternating tetrafluoroethylene–propylene copolymer with a cure site monomer in an aqueous suspension. It is used as an elastomeric surface treatment of various substrates such as metals, ceramics, plastics, other elastomers, textiles, and paper. The incorporated cure site monomer allows this material to be cured using either peroxide systems or electron beam irradiation. Classified by ASTM D 1418-01 as FEPM.

Material Features:

    Heat Resistance*: Mechanical properties of AFLAS do not deteriorate even when used for prolonged exposure to 200°C. AFLAS can be used continuously for 2 to 3 months at 230°C and for 10-30 days at 260°C.
  • Chemical Resistance: Parts fabricated from AFLAS compounds perform well in the amine and base-rich environments commonly found in sour oil and gas exploration, completion and production. In automotive and heavy equipment applications, AFLAS stands up well to attack from amine-containing additives in oils and transmission fluids.
  • Steam Resistance*: Unaffected by extended exposure to 200°C steam.
  • Electrical Properties: Excellent volume resistivity (greater than 1016 O-cm) unmatched by other fluoroelastomers.
  • Radiation Resistance*: Stable up to 2000 kGy of gamma ray radiation.
End User Benefits:
    Improved flexibility
  • Excellent thermal and chemical stability
Typical Applications:
    Coating additives
  • Surface modified parts

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 - 1.20 g/cc
Solids Content 30 - 40 %
Particle Size 20 - 50 µm
pH 3.0 - 10
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 230 °C
 260 °C
 
Descriptive Properties
AppearanceWhite, milky liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC AFLAS® 200P TFE/P Fluoroelastomers
AGC AFLAS® 150P TFE/P Fluoroelastomers
AGC AFLAS® 150L TFE/P Fluoroelastomers
AGC AFLAS® 150E TFE/P Fluoroelastomers
AGC AFLAS® 150CS TFE/P Latex

PAGCX007 / 191116

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.