MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
The NanoSteel® Company SHS 9172 HVOF Steel Alloy, Atomized Powder
Categories: Metal; Ferrous Metal; Alloy Steel; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Coating Description: SHS 9172 HVOF is an iron based steel alloy with a nanoscale microstructure that features exceptional resistance to wear, abrasion, impact, corrosion and high temperature oxidation. SHS 9172 HVOF is also a coating alternative to electrolytic hard chromium.

    Key Performance Characteristics
  • Exceptional abrasion resistance for a metallic material
  • Significant corrosion and high temperature oxidation resistance
  • Coatings provide hardness, corrosion and wear resistance superior to hard chrome
  • Can be finished to very high surface specifications as a replacement for hard chrome

Application Process: High Velocity Oxygen Fuel (HVOF) thermal spraying

Information Provided by The NanoSteel Company, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.59 g/ccCoating Property
Porosity <= 5.0 %Coating Property
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 1000 - 1100kg/mm2; HV300
 
Component Elements PropertiesOriginal ValueComments
Boron, B <= 5.0 %
Carbon, C <= 4.0 %
Chromium, Cr <= 25 %
Iron, Fe >= 28 %
Manganese, Mn <= 3.0 %
Molybdenum, Mo <= 6.0 %
Niobium, Nb (Columbium, Cb) <= 12 %
Silicon, Si <= 2.0 %
Tungsten, W <= 15 %
 
Descriptive Properties
Impact ResistanceNo delamination/cracking at 480 in-lbsDrop Impact Testing
Wear Resistance Mass Loss (g)0.072000 cycles; ASTM G65-04 Procedure B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek RENE® 220 Centri-Vac Nickel Cobalt Based Alloy
HP Alloys Alloy 718, 0% Cold Worked, Not Aged
ATI Wah Chang TI-45 Nb
ATI Allegheny Ludlum Altemp® 718 Nickel-Base Superalloy, Solution Treated plus Precipitation Heat Treated, UNS N07718
The NanoSteel® Company SHS 9172 TWAS Steel Alloy, Cored Wire

NNANO003 / 106798

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.