MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro Desmopan® 3360A DPS 061 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion- and injection molding grade; free from plasticizers; excellent abrasion resistance; good wear resistance; Application; Films; hard - soft systems; Screenpacks

Mechanical property data for samples at 50% RH.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6161ISO 868
Tensile Strength, Ultimate 31.0 MPa4500 psi200 mm/min; DIN 53504
Elongation at Break 938 %938 %200 mm/min; DIN 53504
Tensile Modulus  0.00700 GPa
@Temperature 60.0 °C
1.02 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.0100 GPa
@Temperature 20.0 °C
1.45 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 0.0370 GPa
@Temperature -20.0 °C
5.37 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
50% Modulus 1.60 MPa
@Strain 50 %
1.60 MPa
@Strain 50 %
200 mm/min; DIN 53504
100% Modulus 2.10 MPa
@Strain 100 %
305 psi
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus 3.70 MPa
@Strain 200 %
537 psi
@Strain 200 %
200 mm/min; DIN 53504
Rebound 55 %55 %Resilience; ISO 4662
Tear Strength 41.0 kN/m234 pli500 mm/min; ISO 34-1
Abrasion 3333mm3; ISO 4649 method A
Compression Set  26 %
@Temperature 23.0 °C,
Time 259000 sec
26 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 55 %
@Temperature 70.0 °C,
Time 86400 sec
55 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 210 °C356 - 410 °FInjection
 180 - 210 °C356 - 410 °FExtrusion
Mold Temperature 20.0 °C68.0 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 3060A TPU
Covestro Desmopan® 3378A TPU
Covestro Desmopan® 453 DPS 041 TPU
Covestro Desmopan® 6064A TPU
Covestro Desmopan® 1080AU TPU

PCOVEST0705 / 202488

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.