MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 3060A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Injection molding grade; free from plasticizers; low abrasion; Application; Sports shoe soles; hard - soft systems

Mechanical property data for samples at 50% RH.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.154 g/cc1.154 g/ccISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6262ISO 868
Tensile Strength, Ultimate 28.0 MPa4060 psi200 mm/min; b.o. ISO 527-1,-3
Elongation at Break 800 %800 %200 mm/min; b.o. ISO 527-1,-3
100% Modulus 2.00 MPa
@Strain 100 %
290 psi
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus 3.50 MPa
@Strain 200 %
508 psi
@Strain 200 %
200 mm/min; DIN 53504
Rebound 49 %49 %Resilience; ISO 4662
Tear Strength 33.0 kN/m188 pli500 mm/min; ISO 34-1
Abrasion 4040mm3; ISO 4649 method A
Compression Set  20 %
@Temperature 23.0 °C,
Time 259000 sec
20 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 28 %
@Temperature 70.0 °C,
Time 86400 sec
28 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1, Method C
 45 %
@Temperature 70.0 °C,
Time 86400 sec
45 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 185 - 215 °C365 - 419 °F
Mold Temperature 20.0 °C68.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 3360A DPS 061 TPU
Covestro Desmopan® 453 DPS 041 TPU
Covestro Desmopan® 6064A TPU
Covestro Desmopan® 1080AU TPU
Covestro Desmopan® 1092A TPU

PCOVEST0704 / 202487

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.