MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 1092A TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Injection molding grade; hydrolysis-stabilized; high mechanical strength; very short cycle times; Application; Shift lever balls; Roller tires; Coupling elements; Shoe heels

Mechanical property data for samples at 50% RH.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.211 g/cc1.211 g/ccISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9393ISO 868
Hardness, Shore D 4242ISO 868
Tensile Strength, Ultimate 48.0 MPa6960 psi200 mm/min; DIN 53504
Elongation at Break 600 %600 %200 mm/min; DIN 53504
Tensile Modulus  0.0470 GPa
@Temperature 60.0 °C
6.82 ksi
@Temperature 140 °F
storage; ISO 6721-1,-4
 0.0970 GPa
@Temperature 20.0 °C
14.1 ksi
@Temperature 68.0 °F
storage; ISO 6721-1,-4
 0.755 GPa
@Temperature -20.0 °C
110 ksi
@Temperature -4.00 °F
storage; ISO 6721-1,-4
100% Modulus 8.90 MPa
@Strain 100 %
1290 psi
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus 16.0 MPa
@Strain 200 %
2320 psi
@Strain 200 %
200 mm/min; DIN 53504
Rebound 40 %40 %Resilience; ISO 4662
Tear Strength 100 kN/m571 pli500 mm/min; ISO 34-1
Abrasion 1111mm3; ISO 4649 method A
Compression Set  25 %
@Temperature 23.0 °C,
Time 259000 sec
25 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 27 %
@Temperature 70.0 °C,
Time 86400 sec
27 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1, Method C
 41 %
@Temperature 70.0 °C,
Time 86400 sec
41 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 230 °C410 - 446 °F
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °F
Drying Temperature 110 °C230 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 1085A TPU
Covestro Desmopan® 1080AU TPU
Covestro Desmopan® 2792A GMP TPU
Covestro Desmopan® 1045D TPU
Covestro Desmopan® 453 DPS 041 TPU

PCOVEST0690 / 202473

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.