MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® 545 Hydraulic/Pneumatic Sealant Thread Sealant
Categories: Polymer; Adhesive; Thermoset

Material Notes:
Thread Sealers
Loctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high pressure applications, liquid thread sealants seal instantly for low pressure testing. When fully cured, they seal to the burst strength of most piping systems.

Loctite® Pre-Applied Thread Sealants are dry-to-the-touch films applied to threaded fittings by fitting suppliers and process centers located throughout North America. Pre-applied thread sealants are ideal for OEMs because they can improve speed of assembly and ensure quality by eliminating on-line dispensing of sealants.

Loctite® 545 Hydraulic/Pneumatic Sealant Thread Sealant
A liquid sealant for locking and sealing high pressure fluid power systems with tapered fittings. Contains no fillers and will not foul valves or fluid fitting systems. Seals operating pressures to 10,000 psi.
Recommended Primer: 7649 (N)
Agriculture Canada approved.
Typical Use: Pneumatic Hydraulic Sealant, No Fillers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Viscosity 14000 cP
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -65.0 °F
 
Descriptive Properties
ColorPurple

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Gravi-Tech™ GRV-UR-110-W Polyurethane, PUR
Avient Gravi-Tech™ GRV-UR-080-W Polyurethane, PUR
Avient Edgetek® UR2-40CF/000 BLACK Polyurethane, PUR
Magnesium, Mg; Sand Cast
Magnesium, Mg; Extruded

PLOCT103 / 51839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.