MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Edgetek® UR2-40CF/000 BLACK Polyurethane, PUR
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Filler Content 40 %40 %Carbon Fiber Reinforcement
Linear Mold Shrinkage, Transverse 0.00090 - 0.0030 cm/cm0.00090 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 98.6 MPa14300 psiASTM D638
Tensile Strength, Yield 103 MPa14900 psiASTM D638
Elongation at Break 7.0 - 11 %7.0 - 11 %ASTM D638
Tensile Modulus 9.31 GPa1350 ksi5.1 mm/min; ASTM D638
Flexural Strength 131 MPa19000 psi1.3 mm/min; ASTM D790
Flexural Modulus 7.93 GPa1150 ksi1.3 mm/min; ASTM D790
Izod Impact, Notched 2.70 J/cm5.06 ft-lb/inInjection Molded; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 10000 ohm-cm100 - 10000 ohm-cmASTM D257
Surface Resistance 100 - 10000 ohm100 - 10000 ohmASTM D257
 
Processing PropertiesMetricEnglishComments
Melt Temperature 216 - 238 °C421 - 460 °F
 
Descriptive Properties
FeaturesBalanced Stiffness/Toughness
 Electrically Conductive
FormsPellets
Generic MaterialPUR, Unspecified
Generic NamePolyurethane, Unspecified (PUR, Unspecified)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConsumer Applications
 Industrial Applications
 Medical/Healthcare Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Gravi-Tech™ GRV-UR-110-W Polyurethane, PUR
Avient Gravi-Tech™ GRV-UR-080-W Polyurethane, PUR
Covestro Texin® 970 U Thermoplastic Polyurethanes (TPU)
Chesterton 652 Pneumatic Lubricant & Conditioner
Henkel Loctite® 545 Hydraulic/Pneumatic Sealant Thread Sealant

PH0POL1074 / 145643

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.