MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.

Its broad molecular weight distribution and density successfully combine excellent performance at high extrusion rates with high film strength and sealability.

Main Applications: Eraclene FA 506 can be processed either in blend or in coextrusion. It is possible to use it pure for high rigidity grocery sacks and shopping bags. Usage in blend and/or in coextrusion with LDPE and LLDPE is also recommended for high strength thermo-shrinkable film, as well as for hygienic packaging. The excellent balance between drawability and bubble stability makes Eraclene FA 506 the optimum choice for manufacturing of high quality thin film characterized by outstanding mechanical properties.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.939 g/ccISO 1183
Thickness 10.0 - 50.0 micronsRecommended
Melt Flow 0.60 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 15 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 550 %ISO 527-3
Film Elongation at Break, TD 750 %ISO 527-3
Elmendorf Tear Strength, MD 2.5475 g/micronISO 6383-2
Elmendorf Tear Strength, TD 25.475 g/micronISO 6383-2
Dart Drop Test 150 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 55.0 MPaISO 527-3
Film Tensile Strength at Break, TD 50.0 MPaISO 527-3
1% Secant Modulus, MD 400 MPaISO 527-3
1% Secant Modulus, TD 500 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 129 °CInternal method
Vicat Softening Point 119 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -60.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 3010D Low Density Polyethylene (LDPE), Blow Molding Grade
LyondellBasell Lupolen 3026F Low Density Polyethylene (LDPE), Blown Film Grade
Versalis Clearflex® FF 508 Octene Copolymer Linear Medium Density Polyethylene
Versalis Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion
Versalis Eraclene® FA 706 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion

PENG129 / 124523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.