Lupolen 3026 F is an additivated, low density polyethylene. It contains slip agent. It is characterized by a good melt strength leading to a good bubble stability during blown film extrusion. LyondellBasell customers report that films made from Lupolen 3026 F exhibit a good shrinkage performance. Lupolen 3026 F provides the option to produce films with good optical and mechanical properties. It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications: Bags & Pouches, Food Packaging Film, Lamination Film, Shrink Film Information provided by LyondellBasell. |