MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Lupolen 3026F Low Density Polyethylene (LDPE), Blown Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Lupolen 3026 F is an additivated, low density polyethylene. It contains slip agent. It is characterized by a good melt strength leading to a good bubble stability during blown film extrusion. LyondellBasell customers report that films made from Lupolen 3026 F exhibit a good shrinkage performance.

Lupolen 3026 F provides the option to produce films with good optical and mechanical properties. It is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications: Bags & Pouches, Food Packaging Film, Lamination Film, Shrink Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.927 g/ccISO 1183-1
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
Slip Level 500 ppmErucamide; LYB Method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 12.0 MPaISO 527-1,-2
Film Elongation at Break, MD 300 %ISO 527-1,-3
Film Elongation at Break, TD 600 %ISO 527-1,-3
Tensile Modulus 300 MPaISO 527-1,-2
Coefficient of Friction <= 0.30ISO 8295
Dart Drop Test 120 gF50; ASTM D 1709
Film Tensile Strength at Break, MD 27.0 MPaISO 527-1,-3
Film Tensile Strength at Break, TD 22.0 MPaISO 527-1,-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 114 °Cpeak; ISO 3146
Vicat Softening Point 100 °CA50N; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze <= 7.0 %
@Thickness 0.0500 mm
ASTM D1003
Gloss >= 50 %@ 20°; ASTM D2457
 >= 100 %@ 60°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 220 °CExtrusion Temperature
 
Descriptive Properties
Failure Energy (J/mm)4DIN 53373
Processing MethodBlown Film
Test Specimenfilm, 50µm blown film extruded at 180°C, and a blow up ratio 2.5:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 3010D Low Density Polyethylene (LDPE), Blow Molding Grade
Versalis Eraclene® FC 82 High Density Polyethylene - Blown Film Extrusion
Versalis Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene
Versalis Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene
LyondellBasell Lupolen 3721C High Density Polyethylene (HDPE), Blown Film Grade

PEQT8547 / 220182

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.