MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Scotchkote™ 323 Purple Patch Compound
Categories: Polymer; Thermoset

Material Notes: 3M Scotchkote 323 Purple Patch Compound is an ambient temperature cure, two-part system designed to protect metal, concrete and other surfaces from corrosion and deterioration. Scotchkote 323 Purple Patch Compound is the patch material color matched to 3M Scotchkote Fusion Bonded Epoxy.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/cc
Viscosity 20000 cPPart B
 120000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Abrasion 0.325[g], CS-17 wheels, 1000g load, 5000 cycles wheels resurfaced every 500 cycles; ASTM D4060-95
 
Processing PropertiesOriginal ValueComments
Cure Time 0.433 hour
@Temperature 50.0 °C
Dry to Touch Time; ASTM D1640 clause 7.5.2
 0.650 hour
@Temperature 50.0 °C
Dry to Handle Time; ASTM D1640 clause 7.7.1
 1.75 hour
@Temperature 24.0 °C
Dry to Touch Time; ASTM D1640 clause 7.5.2
 2.65 hour
@Temperature 24.0 °C
Dry to Handle Time; ASTM D1640 clause 7.7.1
 7.00 hour
@Temperature 5.00 °C
Dry to Touch Time; ASTM D1640 clause 7.5.2
 8.00 hour
@Temperature 5.00 °C
Dry to Handle Time; ASTM D1640 clause 7.7.1
Shelf Life 24.0 Month
 
Descriptive Properties
AppearancePurple

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35349 / 170096

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.