MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotchkote™ 323 Purple Patch Compound
Categories: Polymer; Thermoset

Material Notes: 3M Scotchkote 323 Purple Patch Compound is an ambient temperature cure, two-part system designed to protect metal, concrete and other surfaces from corrosion and deterioration. Scotchkote 323 Purple Patch Compound is the patch material color matched to 3M Scotchkote Fusion Bonded Epoxy.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³
Viscosity 20000 cP20000 cPPart B
 120000 cP120000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Abrasion 0.3250.325[g], CS-17 wheels, 1000g load, 5000 cycles wheels resurfaced every 500 cycles; ASTM D4060-95
 
Processing PropertiesMetricEnglishComments
Cure Time  26.0 min
@Temperature 50.0 °C
0.433 hour
@Temperature 122 °F
Dry to Touch Time; ASTM D1640 clause 7.5.2
 39.0 min
@Temperature 50.0 °C
0.650 hour
@Temperature 122 °F
Dry to Handle Time; ASTM D1640 clause 7.7.1
 105 min
@Temperature 24.0 °C
1.75 hour
@Temperature 75.2 °F
Dry to Touch Time; ASTM D1640 clause 7.5.2
 159 min
@Temperature 24.0 °C
2.65 hour
@Temperature 75.2 °F
Dry to Handle Time; ASTM D1640 clause 7.7.1
 420 min
@Temperature 5.00 °C
7.00 hour
@Temperature 41.0 °F
Dry to Touch Time; ASTM D1640 clause 7.5.2
 480 min
@Temperature 5.00 °C
8.00 hour
@Temperature 41.0 °F
Dry to Handle Time; ASTM D1640 clause 7.7.1
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearancePurple

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35349 / 170096

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.