MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed Arlon® 1263 PEEK, Carbon Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprietary manufacturing and machining processes to ensure that Arlons properties consistently outperform the competition.

Greene, Tweed offers several different Arlon materials, and all provide high tensile strength and elongation properties, excellent shear strength and creep resistance, outstanding fatigue resistance, broad chemical and radiation resistance, and no susceptibility to hydrolysis (steam/hot water). Our engineers work one on one with customers to find the right solution for each specific application.

Information provided by Greene Tweed.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Deformation 0.060 %0.060 %ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 108108ASTM D785
Hardness, Shore D 9292ASTM D2240
Tensile Strength at Break 230 MPa33400 psiASTM D368
Elongation at Break 1.9 %1.9 %ASTM D638
Flexural Strength 347 MPa50300 psiASTM D790
Flexural Modulus 19.0 GPa
@Strain 0.5 %
2750 ksi
@Strain 0.5 %
Secant; ASTM D790
Compressive Yield Strength >= 4.14 MPa>= 600 psi
Compressive Strength 262 MPa38000 psiASTM D695
Shear Strength 95.8 MPa13900 psiTransverse; ASTM D732
 120 MPa17400 psiAxial; ASTM D732
Secant Modulus 21.72 GPa3150 ksiTensile 0.5% Secant Modulus; ASTM D638
Coefficient of Friction, Dynamic 0.180.18PV=12600 psi-ft./min.; ASTM G77
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.6 µm/m-°C
@Temperature <=149 °C
7.00 µin/in-°F
@Temperature <=300 °F
ASTM E228
 30.6 µm/m-°C
@Temperature >=149 °C
17.0 µin/in-°F
@Temperature >=300 °F
ASTM E228
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyetherketoneketone (PEKK), Unreinforced
Greene Tweed Arlon® 1286 Polyketone, Carbon Filled
Greene Tweed Arlon® 1555 PEEK, Carbon, Graphite Filled
Overview of materials for Polyetheretherketone, Carbon Fiber Filled

PGREEN53 / 42347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.