MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed Arlon® 1286 Polyketone, Carbon Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Greene Tweed offers precision plastic components for a variety of demanding semiconductor applications. These components are made from a full range of high-performance plastic materials including Arlon® 1286, which is ideal for applications requiring exceptionally high physical properties, wear resistance and chemical compatibility.

Applications:

  • CMP retainer rings
  • Guides
  • Supports

Information provided by Greene Tweed.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.49 g/cc1.49 g/ccASTM D792
Water Absorption 0.10 %0.10 %24 hrs, 73°F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9393ASTM D2240
Tensile Strength at Break 260 MPa37700 psiASTM D368
Elongation at Break 1.3 %1.3 %ASTM D638
Flexural Strength 392 MPa56800 psiASTM D790
Flexural Modulus 27.9 GPa
@Strain 0.5 %
4040 ksi
@Strain 0.5 %
Secant; ASTM D790
Shear Strength 95.98 MPa13920 psiTransverse; ASTM D732
 135.6 MPa19660 psiAxial; ASTM D732
Coefficient of Friction, Dynamic 0.140.14PV=12600 psi-ft./min.; ASTM G77
 
Thermal PropertiesMetricEnglishComments
CTE, linear  0.900 µm/m-°C
@Temperature <=149 °C
0.500 µin/in-°F
@Temperature <=300 °F
ASTM E228
 2.16 µm/m-°C
@Temperature >=149 °C
1.20 µin/in-°F
@Temperature >=300 °F
ASTM E228
Deflection Temperature at 1.8 MPa (264 psi) 316 °C600 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polyetherketoneketone (PEKK), Unreinforced
Greene Tweed Arlon® 1263 PEEK, Carbon Filled
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
Ensinger Tecapeek® Polyetheretherketone (PEEK)

PGREEN54 / 42348

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.