MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Greene Tweed Arlon® 1286 Polyketone, Carbon Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Greene Tweed offers precision plastic components for a variety of demanding semiconductor applications. These components are made from a full range of high-performance plastic materials including Arlon® 1286, which is ideal for applications requiring exceptionally high physical properties, wear resistance and chemical compatibility.

Applications:

  • CMP retainer rings
  • Guides
  • Supports

Information provided by Greene Tweed.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccASTM D792
Water Absorption 0.10 %24 hrs, 73°F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 93ASTM D2240
Tensile Strength at Break 37700 psiASTM D368
Elongation at Break 1.3 %ASTM D638
Flexural Strength 56800 psiASTM D790
Flexural Modulus 4.04e+6 psi
@Strain 0.5 %
Secant; ASTM D790
Shear Strength 13920 psiTransverse; ASTM D732
 19660 psiAxial; ASTM D732
Coefficient of Friction, Dynamic 0.14PV=12600 psi-ft./min.; ASTM G77
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.500 µin/in-°F
@Temperature <=149 °C
ASTM E228
 1.20 µin/in-°F
@Temperature >=149 °C
ASTM E228
Deflection Temperature at 1.8 MPa (264 psi) 600 °F
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for PEKK, Unreinforced
Greene Tweed Arlon® 1263 PEEK, Carbon Filled
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
Ensinger Tecapeek® Polyetheretherketone (PEEK)

PGREEN54 / 42348

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.