MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® 74G33W NC010 PA66+PA6-GF33
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 30% Glass Fiber Reinforced

Material Notes: 33% Glass Reinforced, UV Stabilized, Polyamide 66 + Polyamide 6

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccDAM; ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPa50% RH; ISO 527-1/-2
 194 MPaDAM; ISO 527-1/-2
Elongation at Break 4.0 %DAM; ISO 527-1/-2
 6.0 %50% RH; ISO 527-1/-2
Tensile Modulus 7500 MPa50% RH; ISO 527-1/-2
 10900 MPaDAM; ISO 527-1/-2
Flexural Modulus 8900 MPaDAM; ISO 178
Poissons Ratio 0.3450% RH
 0.34DAM
Charpy Impact Unnotched 95.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 12.3 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 16.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 245 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 225 °CDAM; ISO 75-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 290 °COptimum, Injection
 280 - 300 °CRange, Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °COptimum, Injection
Ejection Temperature 210 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-(PA66+PA6),GF33,M1GL1N,S14-110
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA66+PA6-GF33<ISO 11469
Polymer(PA66+PA6)-GF33
Processing Hold Pressure Time (s/mm)3Injection
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA66+PA6-GF33ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 74G33W BK196 PA66+PA6-GF33
DuPont Mobility and Materials Zytel® 70G30HSL NC010 PA66-GF30
Celanese Zytel® 70G33HS1L BK031 PA66-GF33
Akro-Plastic Akromid® B3 GF 20 2 RM-D (3375) PA 6 Dry, 20% Glass Fiber Filled
Akro-Plastic Akromid® B3 GF 30 2 RM-D black (3424) PA 6 + ABS Dry, 30% Glass Filled

PDSX5366 / 198006

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.