MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Zytel® 70G30HSL NC010 PA66-GF30  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 30% Glass Reinforced, Heat Stabilized, Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³DAM; ISO 1183
Water Absorption 6.0 %
@Thickness 2.00 mm
6.0 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.90 %
@Thickness 2.00 mm
1.90 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 888850% RH; ISO 2039-2
 104104DAM; ISO 2039-2
Hardness, Rockwell R 11711750% RH; ISO 2039-2
 124124DAM; ISO 2039-2
Tensile Strength at Break 130 MPa18900 psi50% RH; ISO 527-1/-2
 200 MPa29000 psiDAM; ISO 527-1/-2
Elongation at Break 3.4 %3.4 %DAM; ISO 527-1/-2
 5.0 %5.0 %50% RH; ISO 527-1/-2
Tensile Modulus 7.00 GPa1020 ksi50% RH; ISO 527-1/-2
 10.0 GPa1450 ksiDAM; ISO 527-1/-2
Flexural Strength 200 MPa29000 psi50% RH; ISO 178
 280 MPa40600 psiDAM; ISO 178
Flexural Modulus 6.30 GPa914 ksi50% RH; ISO 178
 9.00 GPa1310 ksiDAM; ISO 178
Poissons Ratio 0.340.34DAM; ISO 527-1/-2
 0.350.3550%RH; ISO 527-1/-2
Izod Impact, Unnotched (ISO)  10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 7.30 J/cm²
@Temperature -30.0 °C
34.7 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 8.20 J/cm²
@Temperature 23.0 °C
39.0 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 9.30 J/cm²
@Temperature 23.0 °C
44.3 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 6800 MPa986000 psi50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 5100 MPa740000 psi50% RH; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm50% RH; IEC 62631-3-1
 >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 1.00e+13 ohm1.00e+13 ohm50% RH; IEC 62631-3-2
Dielectric Constant  4.1
@Frequency 1e+6 Hz
4.1
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 4.4
@Frequency 100 Hz
4.4
@Frequency 100 Hz
DAM; IEC 62631-2-1
 4.6
@Frequency 1e+6 Hz
4.6
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 10.8
@Frequency 100 Hz
10.8
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Dielectric Strength 32.0 kV/mm813 kV/in50% RH; IEC 60243-1
 38.0 kV/mm965 kV/inDAM; IEC 60243-1
Dissipation Factor  0.0070
@Frequency 100 Hz
0.0070
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.015
@Frequency 1e+6 Hz
0.015
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.065
@Frequency 1e+6 Hz
0.065
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 0.46
@Frequency 100 Hz
0.46
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Comparative Tracking Index 400 V400 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 22.0 µm/m-°C12.2 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 107 µm/m-°C59.4 µin/in-°FDAM; ISO 11359-1/-2
Melting Point 263 °C505 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 261 °C502 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 248 °C478 °FDAM; ISO 75-1/-2
Glass Transition Temp, Tg 20.0 °C68.0 °F10°C/min; 50% RH; ISO 11357-1/-2
 80.0 °C176 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread 13.0 mm/min
@Thickness 1.00 mm
0.512 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 24 %24 %DAM; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 - 305 °C545 - 581 °FInjection
 295 °C563 °FInjection Optimum
Mold Temperature 70.0 - 120 °C158 - 248 °FInjection
 100 °C212 °FInjection Optimum
Ejection Temperature 210 °C410 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiInjection
 
Descriptive Properties
Drying RecommendedyesInjection
Emission of organic compounds6 µgC/gVDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging F-value (refraction) (%)95ISO 6452; DAM
Fogging G-value (condensate) (mg)0.3ISO 6452; DAM
Hold pressure time (s/mm)3Injection
Max. screw tangential speed (m/s)0.2Injection
Odor4.5VDA 270
Part Marking CodePA66-GF30ISO 11469
ProcessingInjection Molding
Regional AvailabilityEurope
 Near East/Africa
Resin IdentificationPA66-GF30ISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 70G30HSL BK039B PA66-GF30
Celanese Zytel® 70G30HSLR BK099 PA66-GF30
Celanese Zytel® 70G30HSLR NC010 PA66-GF30
Celanese Zytel® 70G30L NC010 PA66-GF30
Celanese Zytel® 103HSL NC010 PA66

PDSX5324 / 197964

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.