MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Synthos SPRINTAN™ SLR 4602 Solution Styrene Butadiene Rubber (S-SBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Composition: SPRINTAN® SLR-4602 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. The product has a medium styrene/high vinyl micro structure and a typical glass transition temperature of -25°C. SPRINTAN® SLR-4602 – Schkopau is partially coupled and bears a GENERATION 2 functionalisation for improved polymer/filler interaction with carbon black as well as with silica. A non-staining stabiliser is added in the production.

Application: SPRINTAN® SLR-4602 – Schkopau provides outstanding wet grip/rolling resistance for fuel efficient tyre treads based on silica and/or carbon black. The high-vinyl micro structure makes SPRINTAN® SLR-4602 – Schkopau applicable in summer-, all-season-, as well as in winter tyres. The material can also be used in high-quality technical rubber articles.

Test Formulation (based on IRB7 black):

  • Polymer - 100.0 parts by mass
  • Stearic Acid - 1.50 parts by mass
  • Zinc Oxide - 3.00 parts by mass
  • Carbon Black IRB 7 - 50.0 parts by mass
  • Aromatic Oil - 5.00 parts by mass
  • Sulphur - 1.75 parts by mass
  • Accelerator (CBS) - 1.00 parts by mass

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.930 g/cc
Volatiles 0.20 %
@Treatment Temp. 105 °C,
Time 3600 sec
5 g in hot air oven; ASTM D5668
Mooney Viscosity 63
@Temperature 100 °C
[MU] ML 1+4; ASTM D1646
Ash 0.030 %ASTM D5667
 
Chemical PropertiesOriginal ValueComments
Styrene Content 21 %Bound; ASTM D5775
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 64ASTM D2240
Tensile Strength at Break 21.6 MPa
@Treatment Temp. 145 °C,
Time 2100 sec
Cure; ASTM D412
Elongation at Break 360 %ASTM D412
300% Modulus 0.0174 GPa
@Strain 300 %
ASTM D412
Rebound 26 %Resilience; ISO 4662
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -25.0 °CHR 10 K/min, half height
 
Descriptive Properties
Composition62.1%Vinyl content
Rheometer12.6 mintc (50), ASTM D5289
 19.1 mintc (90), ASTM D5289
 2.5 dNmML, ASTM D5289
 21.6 dNmMH, ASTM D5289
 7.6 mints2, test temperature 160°C; ASTM D5289

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Synthos BUNA™ SB 1502 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Synthos SPRINTAN™ SLR 4601 Solution Styrene Butadiene Rubber (S-SBR)
Synthos BUNA™ SB 1500 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)
Synthos SPRINTAN™ SLR 4630 Solution Styrene Butadiene Rubber (S-SBR)

PZZDWST240 / 142449

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.