MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade; Polystyrene, Transparent Grade

Material Notes: Description: Injection Molding, PS, High Transparency, Heat Resistance

Application: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.

CAS: 9003-53-6-5

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Maximum Moisture Content 0.010Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238 (G)
 28 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238 (I)
 120 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238 (G)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ASTM D785
Tensile Strength, Yield 470 kg(f)/cm²
@Thickness 3.20 mm
50mm/min; ASTM D638
Elongation at Break 4.0 %
@Thickness 3.20 mm
50mm/min; ASTM D638
Tensile Modulus 29100 kg(f)/cm²
@Thickness 3.20 mm
1mm/min; ASTM D638
Flexural Yield Strength 860 kg(f)/cm²
@Thickness 3.20 mm
15mm/min; ASTM D790
Flexural Modulus 33200 kg(f)/cm²
@Thickness 3.20 mm
15mm/min; ASTM D790
Izod Impact, Notched 1.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 1.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 40.0 kV/mm
Arc Resistance 120 - 180 secASTM D495
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=1.50 mm
 15 - 30 sec
@Thickness >=3.00 mm
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness 1.50 mm
 >= 120 arcs
@Thickness 3.00 mm
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Vicat Softening Point 95.0 °C
@Load 5.00 kg
50°C/h; ASTM D1525
UL RTI, Electrical 50.0 °C
@Thickness >=1.50 mm
 50.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 50.0 °C
@Thickness >=1.50 mm
 50.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 50.0 °C
@Thickness >=1.50 mm
 50.0 °C
@Thickness >=3.00 mm
Flammability, UL94 HB
@Thickness >=1.50 mm
 HB
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 170 - 190 °CInjection Molding
Middle Barrel Temperature 180 - 200 °CInjection Molding
Front Barrel Temperature 190 - 210 °CInjection Molding
Nozzle Temperature 190 - 220 °CInjection Molding
Melt Temperature 190 - 220 °CInjection Molding
Mold Temperature 40.0 - 70.0 °CInjection Molding
Drying Temperature 80.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPaInjection Molding
Screw Speed 30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance
A. Schulman ComAlloy Hiloy® 212 Polystyrene, Glass Reinforced
A. Schulman POLYBATCH™ U-7000-HS Blowing Agent Concentrate Based In HIPS

PLAY605 / 148615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.