MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade; Polystyrene, Transparent Grade

Material Notes: Description: Injection Molding, PS, High Transparency, Heat Resistance

Application: PSP, Food Tray, Electric/Electrical Component, Coating

CAS: 9003-53-6

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccASTM D792
Maximum Moisture Content 0.0100.010Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow  3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238 (G)
 8.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
8.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238 (I)
 39 g/10 min
@Load 10.0 kg,
Temperature 220 °C
39 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238 (G)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM D785
Tensile Strength, Yield 52.0 MPa
@Thickness 3.20 mm
7540 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 4.0 %
@Thickness 3.20 mm
4.0 %
@Thickness 0.126 in
50mm/min; ASTM D638
Tensile Modulus 2.88 GPa
@Thickness 3.20 mm
418 ksi
@Thickness 0.126 in
1mm/min; ASTM D638
Flexural Yield Strength 98.1 MPa
@Thickness 3.20 mm
14200 psi
@Thickness 0.126 in
15mm/min; ASTM D790
Flexural Modulus 3.27 GPa
@Thickness 3.20 mm
474 ksi
@Thickness 0.126 in
15mm/min; ASTM D790
Izod Impact, Notched  0.0981 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
0.184 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 0.0981 J/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
0.184 ft-lb/in
@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cm
Dielectric Strength 42.0 kV/mm1070 kV/in
Arc Resistance 120 - 180 sec120 - 180 secASTM D495
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness >=1.50 mm
7.0 - 15 sec
@Thickness >=0.0591 in
 15 - 30 sec
@Thickness >=3.00 mm
15 - 30 sec
@Thickness >=0.118 in
High Amp Arc Ignition, HAI  60 - 120 arcs
@Thickness 1.50 mm
60 - 120 arcs
@Thickness 0.0591 in
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR 25.4 - 50.0 mm/min1.00 - 1.97 in/min
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
@Thickness 6.40 mm
203 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
@Thickness 6.40 mm
190 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 96.0 °C
@Load 5.00 kg
205 °F
@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical  50.0 °C
@Thickness >=1.50 mm
122 °F
@Thickness >=0.0591 in
 50.0 °C
@Thickness >=3.00 mm
122 °F
@Thickness >=0.118 in
UL RTI, Mechanical with Impact  50.0 °C
@Thickness >=1.50 mm
122 °F
@Thickness >=0.0591 in
 50.0 °C
@Thickness >=3.00 mm
122 °F
@Thickness >=0.118 in
UL RTI, Mechanical without Impact  50.0 °C
@Thickness >=1.50 mm
122 °F
@Thickness >=0.0591 in
 50.0 °C
@Thickness >=3.00 mm
122 °F
@Thickness >=0.118 in
Flammability, UL94  HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
 HB
@Thickness >=3.00 mm
HB
@Thickness >=0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 170 - 190 °C338 - 374 °FInjection Molding
Middle Barrel Temperature 180 - 200 °C356 - 392 °FInjection Molding
Front Barrel Temperature 190 - 210 °C374 - 410 °FInjection Molding
Nozzle Temperature 190 - 220 °C374 - 428 °FInjection Molding
Melt Temperature 190 - 220 °C374 - 428 °FInjection Molding
Mold Temperature 40.0 - 70.0 °C104 - 158 °FInjection Molding
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPa4260 - 8530 psiInjection Molding
Screw Speed 30 - 60 rpm30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance
Total PSC 1960N Crystal Polystyrene
LG Chemical BM662 ABS, Heat Resistance

PLAY607 / 148617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.