MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M PM-4800 Stain Resistant Additive and Sealer
Categories: Fluid

Material Notes: Introduction: 3M™ Stain Resistant Additive and Sealer PM-4800 is a fluorochemical resin concentrate in ethyl acetate designed for industrial application to porous hard surfaces such as concrete, marble, terracotta, etc. Properly applied, PM- 4800 additive imparts excellent and durable water, oil and stain repellent properties as well as dirt pick-up resistance on all types of porous hard surfaces. The substrate’s natural characteristics are generally unaffected by the application of this product. Be sure to evaluate the 3M product for compatibility in your particular application before using.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.995 g/cc0.0359 lb/in³
Solids Content 40 %40 %
 
Thermal PropertiesMetricEnglishComments
Boiling Point 77.0 °C171 °F
Flash Point -4.00 °C24.8 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Monthfrom date of manufacture
 
Descriptive Properties
AppearanceClear yellow liquid
Composition0.6Ethyl acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M SRC-220 Stain Resistant Additive

PMM40003 / 194894

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.