MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M SRC-220 Stain Resistant Additive
Categories: Fluid; Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Product Description: 3M™ Stain Resistant Additive SRC-220 is an aqueous fluorinated polyurethane dispersion (PUD) that, when formulated as a penetrating sealer, adds stain resistance and release, and water and oil repellency characteristics to porous surfaces. The SRC-220 concentrate can also be used as an additive to many general coating formulations, and to various construction materials. This product is suitable for both indoor and outdoor use.

Suggested Applications: SRC-220 additive can be diluted using water, water-miscible solvents (such as alcohols, ketones, ethylene-glycol-monobutyl-ether, dipropylene glycol monomethyl ether and other glycol mono- or di- ethers), and water-solvent mixtures. When applied at a 2 to 5% concentration and used as a penetrating sealer, SRC-220 additive provides water and oil repellency and stain resistance to porous surfaces such as concrete, grout, unglazed tile, granite, clay, slate, limestone and terra cotta. The sealer is easily applied, dries quickly, is durable and causes no significant change to the appearance of the treated surface. Laboratory tests show that repellency and stain resistance improves when SRC-220 additive is diluted with a water-miscible solvent or a water/solvent mixture, as compared to dilution with water only.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0398 lb/in³
Volatile Organic Compounds (VOC) Content <= 240 g/l<= 240 g/lASTM 3960-89
pH 7.0 - 8.07.0 - 8.0
Viscosity <= 30 cP<= 30 cP
Vapor Pressure 0.0240 bar18.0 torr
 
Thermal PropertiesMetricEnglishComments
Boiling Point 100 °C212 °F
Flash Point >= 93.3 °C>= 200 °F
 
Descriptive Properties
AppearanceSlightly translucent solution

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M PM-4800 Stain Resistant Additive and Sealer
3M PM-1680 Stain Resistant Additive and Sealer

PMM40005 / 194896

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.