MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M PM-1680 Stain Resistant Additive and Sealer
Categories: Fluid

Material Notes: 3M™ Stain Resistant Additive and Sealer PM-1680 is a water dilutable general purpose fluorochemical emulsion designed for application to porous hard surfaces, such as terracotta, grout, marble and concrete. Properly applied, PM-1680 additive imparts excellent water, oil and stain repellent properties as well as dirt pick-up resistance to these substrates. The substrate’s natural characteristics (color, breathability) are generally unaffected by the application of this product. PM-1680 additive is a water-based product, and can be used as an ingredient in a wide variety of products or industrially-applied formulations.

Information provided by 3M™

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.995 - 1.10 g/cc0.0359 - 0.0398 lb/in³
Solids Content 26 - 28 %26 - 28 %
pH 4.0 - 7.04.0 - 7.0
 
Processing PropertiesMetricEnglishComments
Moisture Content 72 - 74 %72 - 74 %
Shelf Life 24.0 Month24.0 Monthfrom date of manufacture
 
Descriptive Properties
AppearanceWhite emulsion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M SRC-220 Stain Resistant Additive

PMM40002 / 194893

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.