MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

P & P Technology CB 70 Carbon Loaded Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Applications: Electrically conductive grades which when properly catalyzed can be considered for applications requiring conductivity such as EMI gaskets, conductive sheaths for ignition cable core, electronic keyboard contacts, etc.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/ccDIN 53479-A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7373DIN 53505-A
Tensile Strength 6.00 MPa870 psiDIN 53504-S1
Elongation at Break 210 %210 %DIN 53504-S1
Tear Strength 12.0 kN/m68.5 pliASTM D624B
Compression Set 33 %33 %DIN ISO815-B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.5 ohm-cm1.5 ohm-cmDIN IEC93

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 3-4170 DIELECTRIC GEL KIT
Wacker LumisilĀ® LR 7601/80 Liquid Silicone Rubber
Chosun Refractories SCX-70 I Special SiC Castable
Chosun Refractories AMC-70 Alumina Magnesia Carbon Bricks for Ladle Wall And Bottom
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2

PPPTEC002 / 133466

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.