MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: DN 70 is a ZTA Alumina Toughened Zirconia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.01 g/cc0.145 lb/in³DIN EN 623-2
Water Absorption 0.00 %0.00 %Open Porosity; DIN EN 623-2
Permeability 0.000.00%, Gas
Weibull Modulus 1010DINV ENV 843-5
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 17001700HV1; DINV ENV 843-4
Tensile Modulus 360 GPa52200 ksiYoung's; DINV ENV 843-2
Flexural Strength 450 MPa65300 psiDIN EN 843-1
Compressive Strength 2700 MPa392000 psiDIN 51067T1
Poissons Ratio 0.230.23DINV ENV 843-2
Fracture Toughness 4.40 MPa-m½4.00 ksi-in½KIC (SEVNB); DIN CEN/TS 14425-1
Shear Modulus 146 GPa21200 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  500000 ohm-cm
@Temperature 400 °C
500000 ohm-cm
@Temperature 752 °F
IEC 672-1
 1.00e+14 ohm-cm
@Temperature 20.0 °C
1.00e+14 ohm-cm
@Temperature 68.0 °F
IEC 672-1
Dielectric Constant 10
@Frequency 1e+6 Hz
10
@Frequency 1e+6 Hz
IEC 672-1
Dielectric Strength 16.0 kV/mm406 kV/inIEC 672-1
Dielectric Loss Index 0.0040
@Frequency 9.00e+9 Hz
0.0040
@Frequency 9.00e+9 Hz
IEC 672-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear  7.00 µm/m-°C
@Temperature 20.0 - 400 °C
3.89 µin/in-°F
@Temperature 68.0 - 752 °F
DIN EN 821-1
 9.00 µm/m-°C
@Temperature 20.0 - 1000 °C
5.00 µin/in-°F
@Temperature 68.0 - 1830 °F
DIN EN 821-1
Specific Heat Capacity 0.800 J/g-°C0.191 BTU/lb-°FDINV ENV 821-3
Thermal Conductivity 15.0 W/m-K104 BTU-in/hr-ft²-°FDIN EN 821-2
Maximum Service Temperature, Air 1500 °C2730 °F
Maximum Service Temperature, Inert 1500 °C2730 °F
 
Descriptive Properties
Ra = Arithmetic Mean Roughness Value (µm)<0.15
Thermal Shock Resistance R1 (K)134calculated; R1 = [σs (1-µ)] / (α·E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
CeramTec ZN 40 Zirconia, ZrO2-MgO
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2
CeramTec MZ 429 Zirconia, ZrO2-Y2O3
CeramTec 848 Zirconia, ZrO2•MgO

CCERA908 / 107508

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.