Description: Lupranate® 223 Isocyanate is a low viscosity derivative of both pure-MDI and polymeric-MDI. With a functionality of approximately 2.2, this isocyanate can be formulated into applications that require good flow and working time such as 1- and 2-component adhesives and coatings.Information provided by BASF |