MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution Luran® S Q440 ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes: Luran S Q440 is a low gloss extrusion ASA grade with excellent weatherability. Luran S Q440 is especially suited for the building and construction market as a low gloss weatherable cap layer. It is provided with a base loading of TiO2 to help in the coloring of the product with a color concentrate. How dark the final application is determines the level of TiO2 in a grade. The data representable is based on 0.125" thick extruded sheets in the cross flow direction.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Melt Flow 4.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
4.0 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM Test
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 33.0 MPa4790 psi2 in/min; ASTM Test
Elongation at Yield 2.6 %2.6 %2 in/min; ASTM Test
Tensile Modulus 1.79 GPa260 ksiASTM Test
Flexural Strength 52.0 MPa7540 psiASTM Test
Flexural Modulus 1.82 GPa264 ksiASTM Test
Izod Impact, Notched 0.540 J/cm
@Temperature -30.0 °C
1.01 ft-lb/in
@Temperature -22.0 °F
ASTM Test
 0.960 J/cm
@Thickness 3.17 mm
1.80 ft-lb/in
@Thickness 0.125 in
ASTM Test
Dart Drop, Total Energy 15.0 J11.1 ft-lbASTM Test
Instrumented Impact Energy at Peak 10.0 J7.38 ft-lbInstrumented Dart Impact (Energy at Peak Force); ASTM Test
 
Thermal PropertiesMetricEnglishComments
CTE, linear 79.0 µm/m-°C
@Temperature -30.0 - 70.0 °C
43.9 µin/in-°F
@Temperature -22.0 - 158 °F
ASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °Fannealed; ASTM Test
Vicat Softening Point 88.0 °C190 °FRate "A" Loading 2 (50 degC/h 50N); ASTM Test
 
Optical PropertiesMetricEnglishComments
Gloss 21 %21 %60° Specular; ASTM Test
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedYes
Primary Processing TechniqueExtrusion
ProcessingOther Extrusion
 Profile Extrusion
 Sheet Extrusion
 Thermoforming
Special characteristicHeat stabilized or stable to heat
 Light stabilized or stable to light
 U.V. stabilized or stable to weather

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Luran® S 757G ASA
INEOS Styrolution Luran® S 778T ASA
INEOS Styrolution Luran® S 777K ASA
INEOS Styrolution Luran® S 776SE ASA
INEOS Styrolution Luran® S 797SE ASA

PBASF9008 / 84772

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.