MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nilit Polynil® P50FI Internally Lubricated Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Description: Polynil P50 FI is an internally lubricated NYLON 66 with excellent flow characteristics and high elongation. It is widely used throughout many industries for applications that have long, thin flow lengths, like cable ties, connectors or industrial components.

Key characteristics:

  • Excellent flow
  • High elongation
  • Good mould release
  • High toughness
  • Good thermal performance
  • UL 94 V2 listed at 0.75 mm

Information provided by NILIT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 1.5 %1.5 %24h in H2O; sim. ISO 62
Water Absorption at Saturation 8.5 %8.5 %sim. ISO 62
Loss On Ignition 28 %28 %ASTM D2863
Viscosity Measurement 5050relative viscosity (formic acid); ASTM D789
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/inNilit
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 81.01 MPa11750 psiASTM D638
Elongation at Break 49 %49 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 2.83 GPa410 ksiASTM D638
Flexural Strength 122 MPa17700 psiASTM D790
 30.0 MPa
@Temperature 90.0 °C
4350 psi
@Temperature 194 °F
ASTM D790
Flexural Modulus 2.85 GPa413 ksiASTM D790
 0.800 GPa
@Temperature 90.0 °C
116 ksi
@Temperature 194 °F
ASTM D790
Izod Impact, Notched (ISO) 5.46 kJ/m²2.60 ft-lb/in²ASTM D256
 4.41 kJ/m²
@Temperature -30.0 °C
2.10 ft-lb/in²
@Temperature -22.0 °F
ASTM D256
Charpy Impact Unnotched NBNBISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.0 kV/mm
@Thickness 2.00 mm
457 kV/in
@Thickness 0.0787 in
ASTM D149
Comparative Tracking Index >= 600 V>= 600 VUL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 225 °C437 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FASTM D648
Vicat Softening Point 240 °C464 °F49 N; ASTM D1525
 255 °C491 °F9.8 N; ASTM D1525
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 
Descriptive Properties
Heat Resistance - Ball TestOKat 125°C, IEC 309
 OKat 165°C, IEC 309

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nilit Polynil® P50N Nucleated Nylon 66
BASF Ultramid® A4H PA66 (Dry)

PLBN08 / 50397

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.