Description: Polynil P50 FI is an internally lubricated NYLON 66 with excellent flow characteristics and high elongation. It is widely used throughout many industries for applications that have long, thin flow lengths, like cable ties, connectors or industrial components. Key characteristics: - Excellent flow
- High elongation
- Good mould release
- High toughness
- Good thermal performance
- UL 94 V2 listed at 0.75 mm
Information provided by NILIT. |