MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zhejiang Juner PC/ABSz-4 Alloy  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Applications: Shell of Small Household Electric Appliance

Information provided by Zhejiang Juner New Materials Co, Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccGB/1033
Water Absorption 0.30 %GB/T1034
Linear Mold Shrinkage 0.0050 - 0.0060 cm/cmGB/15585
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 52.0 MPaGB/1040
Flexural Strength 82.0 MPaGB/9341
Charpy Impact Unnotched NBIS0179-1:2000
Charpy Impact, Notched 4.50 J/cm²IS0179-1:2000
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmD257
Comparative Tracking Index 200 VGB/4207
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 100 °CGB/1634
Flammability, UL94 HB - V-0GB/T2408
 
Processing PropertiesOriginal ValueComments
Processing Temperature 225 - 270 °C
Drying Temperature 100 °C
@Time 14400 sec
Chute Hot-Wind
 100 °C
@Time 18000 sec
Horizontal Oven
Injection Pressure 50.0 - 100 MPa
 
Descriptive Properties
Chromatism (?E)=0.8
Granule DiameterΦ3x3-5
Speed of Shoot, %35-80
Surface PolishHigh
WeatherabilityAdjustive

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accuguard ABS ABS860V0L Flame Retardant
Covestro Bayblend® T65 XF Polycarbonate + ABS
Ecomass® 720ZD91 Tungsten Filled ABS
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade
A. Schulman Diamond DIAMALOY ST4600 TPE/ABS Alloy, Soft Touch Resin

PJUNER48 / 48561

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.