System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Zhejiang Juner PC/ABSz-4 Alloy
(discontinued **)
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Polycarbonate/ABS Alloy, Unreinforced
;
Polycarbonate (PC)
Material Notes:
Applications: Shell of Small Household Electric Appliance
Information provided by Zhejiang Juner New Materials Co, Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.21
g/cc
0.0437
lb/in³
GB/1033
Water Absorption
0.30 %
0.30 %
GB/T1034
Linear Mold Shrinkage
0.0050
-
0.0060
cm/cm
0.0050
-
0.0060
in/in
GB/15585
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
52.0
MPa
7540
psi
GB/1040
Flexural Strength
82.0
MPa
11900
psi
GB/9341
Charpy Impact Unnotched
NB
NB
IS0179-1:2000
Charpy Impact, Notched
4.50
J/cm²
21.4
ft-lb/in²
IS0179-1:2000
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.00e+17
ohm-cm
1.00e+17
ohm-cm
D257
Comparative Tracking Index
200
V
200
V
GB/4207
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
100
°C
212
°F
GB/1634
Flammability, UL94
HB - V-0
HB - V-0
GB/T2408
Processing Properties
Metric
English
Comments
Processing Temperature
225
-
270
°C
437
-
518
°F
Drying Temperature
100
°C
@Time 14400 sec
212
°F
@Time 4.00 hour
Chute Hot-Wind
100
°C
@Time 18000 sec
212
°F
@Time 5.00 hour
Horizontal Oven
Injection Pressure
50.0
-
100
MPa
7250
-
14500
psi
Descriptive Properties
Chromatism (?E)
=0.8
Granule Diameter
Φ3x3-5
Speed of Shoot, %
35-80
Surface Polish
High
Weatherability
Adjustive
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Aclo Accuguard ABS ABS860V0L Flame Retardant
Covestro Bayblend® T65 XF Polycarbonate + ABS
Ecomass® 720ZD91 Tungsten Filled ABS
Bhansali Engineering Abstron IM-14G ABS Very High Rigidity Injection Molding Grade
A. Schulman Diamond DIAMALOY ST4600 TPE/ABS Alloy, Soft Touch Resin
PJUNER48 / 48561
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.