MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bostik 6332 Quick Setup EVA Glue Stick
Categories: Polymer; Adhesive; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Bostik 6332 Quick Setup EVA Glue Stick
Short open time and quick set up. Low viscosity. Easy to gun. Withstands elevated temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 2000 cP
@Temperature 177 °C
2000 cP
@Temperature 350 °F
Typical
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 77.2 °C171 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 0.15 - 0.20 min0.15 - 0.20 minOpen Time
 
Descriptive Properties
ColorStraw / opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Valley Adhesives EM-422 High Temperature Application Glue Stick
Parson Adhesives PARLITE® 4760 UV Glue and UV Adhesive for Electronic Assembly
Chemical Concepts H2O Glue® Aquabonder Underwater Adhesive
Bostik 2385 General Purpose EVA Glue Stick
Bostik 1525 Medium Performance, Oil Resistant Polyamide Glue Stick

PBOST23 / 27582

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.