MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parson Adhesives PARLITE® 4760 UV Glue and UV Adhesive for Electronic Assembly
Categories: Polymer; Adhesive

Material Notes: Application: Potting, Encapsulating, bonding of electronic parts.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 40000 - 60000 cP40000 - 60000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5252
Tensile Strength 8.27 MPa1200 psi
Elongation at Break 48 %48 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TW200F6 PA46-GF30, Dry, 30% Glass Filled, Heat Stabilized
Envalior Stanyl® TE250F6 PA46-GF30 FR(17), Dry, 30% Glass Filled, Heat Stabilized, Flame Retardant
Parson Adhesives PARLITE® 4725 UV Glue and UV Adhesive for Electronic Assembly
Envalior Stanyl® 46HF5041LW PA46-GF40 FR(17), Conditioned, 40% Glass Filled, Heat Stabilized, Flame Retardant
Overview of materials for Methacrylate Adhesive

PPARSN085 / 186528

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.