MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.500 - 1.50 g/cc0.0181 - 0.0541 lb/in³Average value: 1.04 g/cc Grade Count:145
Volatile Organic Compounds (VOC) Content 10.0 - 20.0 g/l10.0 - 20.0 g/lAverage value: 11.3 g/l Grade Count:15
Viscosity 5.00 - 2.00e+6 cP5.00 - 2.00e+6 cPAverage value: 160000 cP Grade Count:193
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60.0 - 75.060.0 - 75.0Average value: 66.5 Grade Count:10
Tensile Strength, Ultimate 0.0276 - 40.0 MPa4.00 - 5800 psiAverage value: 18.0 MPa Grade Count:121
 0.0965266 - 0.0965266 MPa
@Temperature 18.3 - 149 °C
14.0000 - 14.0000 psi
@Temperature 65.0 - 300 °F
Average value: 0.0965 MPa Grade Count:1
Elongation at Break 5.00 - 300 %5.00 - 300 %Average value: 78.0 % Grade Count:125
Elongation at Yield 15.0 - 70.0 %15.0 - 70.0 %Average value: 36.3 % Grade Count:8
Modulus of Elasticity 0.0689 - 1.90 GPa10.0 - 275 ksiAverage value: 0.665 GPa Grade Count:66
Shear Strength 0.0345 - 32.0 MPa5.00 - 4640 psiAverage value: 8.91 MPa Grade Count:78
Adhesive Bond Strength 0.600 - 31.0 MPa87.0 - 4500 psiAverage value: 18.6 MPa Grade Count:109
Tensile Impact Strength 35.7 - 46.2 kJ/m²17.0 - 22.0 ft-lb/in²Average value: 41.3 kJ/m² Grade Count:9
Tensile Impact >= 8.0085 J/cm
@Temperature -40.0 - -40.0 °C
>= 15.003 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 8.01 J/cm Grade Count:1
Peel Strength 1.75 - 11.4 kN/m10.0 - 65.0 pliAverage value: 4.96 kN/m Grade Count:20
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.0000800 - 100 µm/m-°C0.0000444 - 55.6 µin/in-°FAverage value: 77.2 µm/m-°C Grade Count:43
Specific Heat Capacity 0.300 J/g-°C0.0717 BTU/lb-°FAverage value: 0.300 J/g-°C Grade Count:41
Thermal Conductivity 0.100 - 0.100 W/m-K0.694 - 0.694 BTU-in/hr-ft²-°FAverage value: 0.100 W/m-K Grade Count:41
Maximum Service Temperature, Air 49.4 - 450 °C121 - 842 °FAverage value: 133 °C Grade Count:150
Minimum Service Temperature, Air -65.0 - -40.0 °C-85.0 - -40.0 °FAverage value: -50.8 °C Grade Count:144
Flash Point -12.8 - 103 °C9.00 - 217 °FAverage value: 44.0 °C Grade Count:119
 
Processing PropertiesMetricEnglishComments
Processing Temperature 18.3 - 29.4 °C65.0 - 85.0 °FAverage value: 24.7 °C Grade Count:7
Cure Time 1.50 - 2880 min0.0250 - 48.0 hourAverage value: 321 min Grade Count:110
Pot Life 1.00 - 130 min1.00 - 130 minAverage value: 22.1 min Grade Count:137
 45.0 - 45.0 min
@Temperature 95.0 - 95.0 °C
45.0 - 45.0 min
@Temperature 203 - 203 °F
Average value: 45.0 min Grade Count:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Cyanoacrylate Adhesive
Overview of materials for Epoxy Adhesive
Overview of materials for Epoxy Adhesive, Flexible
Overview of materials for Epoxy, Electrically Conductive
Overview of materials for Thermoset Polyurethane, Adhesive

O1390 / 77877

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.