MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase Nylex™ 2185 FR V0 Polyamide + PP
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polypropylene (PP)

Material Notes:

Features:

  • Crack Resistance, Good
  • Dimensional Stability, Good
  • Impact Resistance, Good
  • Moisture Resistant
  • Processability, Good
  • Flame Retardant
  • Forms:

  • Pellets
  • Processing Methods:

  • Injection Molding
  • Uses:

  • Electrical Parts
  • Housing, Electrical
  • Safety Equipment
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.22 g/cc1.22 g/ccASTM 792
    Linear Mold Shrinkage 0.0090 cm/cm0.0090 in/inASTM D955
    Melt Flow 1.0 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    1.0 g/10 min
    @Load 4.76 lb,
    Temperature 446 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate 42.7 MPa6200 psiASTM D638
    Elongation at Break 40 %40 %ASTM D638
    Flexural Strength 42.7 MPa6200 psiASTM D790
    Flexural Modulus 1.52 GPa220 ksiMethod I (3 point load), Procedure B); ASTM D790
    Izod Impact, Notched 0.667 J/cm1.25 ft-lb/inASTM D256
    Gardner Impact 14.12 J10.42 ft-lbASTM D3029
     
    Thermal PropertiesMetricEnglishComments
    Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C201 °FUnannealed; ASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 52.8 °C127 °FUnannealed; ASTM D648
    Vicat Softening Point 166 °C331 °FASTM D1525
    Flammability, UL94 V-0V-0

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant
    Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant
    Elastocon TPE Technologies Elastocon® 8068N Thermoplastic Elastomer
    Mapal Plastics Maplon CFA-HK Polypropylene Sheet
    Multibase Multi-Flam™ 0206 PP Polypropylene

    PMULTI125 / 54029

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.