Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms: PelletsProcessing Methods: Injection MoldingUses: Electrical PartsHousing, Electrical Safety EquipmentInformation provided by Multibase |