MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Ertalyte™ TX Internally Lubricated Semi-Crystalline PET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Ertalyte™ TX Polyethylene Terephthalate Polyester PET is an a premium internally lubricated bearing, semi-crystalline grade that exhibits superior dimensional stability, excellent wear resistance, a low coefficient of friction, high strength and rigidity, outstanding stain resistance, and great chemical and abrasion resistance.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.44 g/ccASTM D792
Water Absorption at Saturation 0.470 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 94.0ASTM D785
Hardness, Shore D 78.0ISO 868
Tensile Strength 76.0 MPaISO 527-1/-2 (7)
Elongation at Yield 4.00 %ISO 527-1/-2 (7)
Flexural Strength 122 MPaISO 178 (12)
Compressive Yield Strength 31.0 MPa
@Strain 1.00 %
ISO 604 (10)
 60.0 MPa
@Strain 2.00 %
ISO 604 (10)
 102 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 59.0 MPaASTM D732
Charpy Impact, Notched 2.50 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 3.60
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 21.0 kV/mmIEC 60243-1 (15)
 533 kV/inASTM D149
Dissipation Factor 0.0200
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µin/in-°FASTM E-831 (TMA)
 65.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 85.0 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.290 W/m-K
 1.90 BTU-in/hr-ft²-°F
Melting Point 491 °FASTM D3418
Maximum Service Temperature, Air 210 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 180 °FASTM D648
Minimum Service Temperature, Air -20.0 °C
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Acceptable
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Unacceptable
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Unacceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ertalyte™ PET Polyester-semi-crystalline thermoplastic, extruded
Cast Nylons Nycast® 6MPY Plasticized Nylon 6
Mitsubishi Chemical Advanced Materials Fluorosint™ 207 PTFE, Compression Molded Synthetic Mica-filled PTFE
Isoflon PETP Polyethylene terephthalate
Mitsubishi Chemical Advanced Materials TIVAR™ 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material

P1SM08 / 20079

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.